Aluminium alloy | 6063,6061,6005,6463,7075etc |
Temper | T3-T8 |
Thickness | General profiles thickness: 0.8 - 5.0 mm Anodized protection thickness: 8 - 25 um Powder coating color thickness: 60 - 120 um |
Length | 4m to 6m per piece, customized length. |
Shape | square, flat, round, hollow, oval, triangle, U-profiles, L-profiles, T-profiles, H-profiles, custom |
Finishing | mill, anodized, powder coated, electrophoresis, wood grain, timber, PVDF paint, polish, brushed |
Color | Metal silver, champagne, black, white, mirror, custom |
Application | windows and doors, curtain walls, glass wall, furniture, ceiling, kitchen, LED strip, vehicles, motor housing, machine, tent, solar. Industrial profile, decoration profile |
Deep Process | CNC, drilling, milling, cutting, welding, bending, assembling |
Production Capacity | 5000 tons monthly |
Certificate and Standard | ISO9001-2008/ISO 9001:2008 CQM Certification SGS, CE, BV, JIS, AS, NZS, QUALICOAT, QUOLANOD available |
Guarantee | Surface color can be stable for 10~20 years indoor using |
GB15763.3,Chinese standard.
EN12543,European standard
EN12600,European standard.
ANSI Z97.1,American standard.
AS/NZS 2208,Australian standard.
Q1: How to judge the quality of float glass?
A1: Flatness, transparency, colorless, impurities, bubbles, etc.
Q2: How to reduce the self-implosion?
A2: The high quality float method is used for hot dip treatment, edge treatment and proper stress intensity. Pay attention to avoid side collision of glass during installation.
Q3: Scope of use of toughened glass?
A3: Safety is not involved in some parts of the building, but it is necessary to install toughened glass to improve the compressive strength and explosion-proof capacity,not to endanger the person safety
Q4: When toughened glass is broken, is the grain smaller the better?
A4: No, the smaller the particle, the easier it is to explode.
Q5: Can toughened glass and semi-toughened glass be made into laminated glass?
A5: Can't. The national standard stipulates: the glass that stresses the difference cannot make laminated glass, because in use process, the pressure that two pieces of glass bears is different.
Q6: Whether the laminated glass can fire, can the sound insulation?
A6: No, the smaller the particle, the easier it is to explode.
Q7: How many uv low-e glass can reduce?
A7: It is not fireproof glass, but has certain fireproof ability, also can soundproof, laminated glass is inside whole sound wave frequency range, in control noise is very good.
Q8: Does the air in the insulating glass do not oxidize the membrane?
A8: No, because there is a molecular sieve in the insulating glass, and the molecular sieve always keeps the air dry, so the membrane is not oxidized.
Q9: How much ultraviolet radiation can low-e glass reduce?
A9: It can reduce uv by 14% compared to heat reflecting glass. That's a 25 percent reduction in uv radiation compared to white glass.