Hot-melt glass/cast glass is also called crystal three-dimensional art glass or Ssgging glass. Hot-melt glass belongs to glass
Product | 3-19mm | Hot melt glass, engraving glass | |||||
Glass thickness | 2440*6000mm | 3mm-30mm | |||||
Glass color | Clear, Ultra clear, French green, Dark green, Euro grey, Dark grey, Ford blue, Dark blue, Ocean blue, Euro bronze, Dark bronze, Golden, Pink, Yellow, etc. | Clear, bronze, grey, blue, green, etc | |||||
Glass process | Flat polish, pencil polish, miter, bevel, O.G. bull nose and etc | ||||||
Max Size | windows and doors in architecture | 12.5x3m or customer's request size | |||||
Payment | 30% deposit, 70% after B/L copy | ||||||
Package | Sea worthy wooden crate with interlayer paper | ||||||
Delivery time | 15-20days | ||||||
Advantage | Hot-melt glass has obvious advantages, rich patterns, strong three-dimensional sense, gorgeous decoration, and dazzling glory. It solves the monotonous dull feeling of ordinary decorative glass facades and makes the glass surface have a vivid shape, which meets people's diverse and aesthetic style pursue. | ||||||
Application | Can be used to make living room TV and sofa background wall, door and window glass, partitions, entrance lights everywhere. |
GB15763.3,Chinese standard.
EN12543,European standard
EN12600,European standard.
ANSI Z97.1,American standard.
AS/NZS 2208,Australian standard.
Q1: How to judge the quality of float glass?
A1: Flatness, transparency, colorless, impurities, bubbles, etc.
Q2: How to reduce the self-implosion?
A2: The high quality float method is used for hot dip treatment, edge treatment and proper stress intensity. Pay attention to avoid side collision of glass during installation.
Q3: Scope of use of toughened glass?
A3: Safety is not involved in some parts of the building, but it is necessary to install toughened glass to improve the compressive strength and explosion-proof capacity,not to endanger the person safety
Q4: When toughened glass is broken, is the grain smaller the better?
A4: No, the smaller the particle, the easier it is to explode.
Q5: Can toughened glass and semi-toughened glass be made into laminated glass?
A5: Can't. The national standard stipulates: the glass that stresses the difference cannot make laminated glass, because in use process, the pressure that two pieces of glass bears is different.
Q6: Whether the laminated glass can fire, can the sound insulation?
A6: No, the smaller the particle, the easier it is to explode.
Q7: How many uv low-e glass can reduce?
A7: It is not fireproof glass, but has certain fireproof ability, also can soundproof, laminated glass is inside whole sound wave frequency range, in control noise is very good.
Q8: Does the air in the insulating glass do not oxidize the membrane?
A8: No, because there is a molecular sieve in the insulating glass, and the molecular sieve always keeps the air dry, so the membrane is not oxidized.
Q9: How much ultraviolet radiation can low-e glass reduce?
A9: It can reduce uv by 14% compared to heat reflecting glass. That's a 25 percent reduction in uv radiation compared to white glass.